DATE:2020-07-07
1 The powder is usded for electrical heating tube of stainless steel with air as the heating mediam and nitrided at 1050 0C (blackened)
2 The powder when tubed and annealed at 1050 0C for 25 minuts, will show white while the sufrace is cut
3 The electrical properties is stable and good in thermal state